Advantages

REACH AZP-908 is an activated AZG superfine powder, and is very popular in this product form. It provides clinical strength protection against wetness and odor.

Details
Formula ID:
A-1017-01
Procedure
  1. Combine Phase A, B and C and heat to 85°C or until clear. Cool to 70°C.
  2. Separately heat Phase D to 70°C and add to step 1.
  3. At 70°C add Phase E and F while mixing
  4. Add Phase G and mix well. Cool to 40°C and transfer to Hobart mixer pot.
  5. Add Phase H slowly while mixing. Add Phase I.
  6. Mix for 15 minutes at low speed, then at moderate speed for 15 minutes.
Ingredient Supplier %w/w
Hydrogenated Castor Oil (Castor Wax MP80) Caschem 2.60
Ingredient Supplier %w/w
Polydecene (Silkflo 364 NF) Lipo 9.00
Ingredient Supplier %w/w
PPG-14 Butyl Ether (Fluid AP) Amerchol 9.00
Ingredient Supplier %w/w
Cyclomethicone (DC 245 Fluid) Dow Corning 44.90
Ingredient Supplier %w/w
Talc 5351L (Whittaker) Whittaker, Clark & Daniels 6.00
Ingredient Supplier %w/w
Enhance Efficacy Aluminum Zirconium Tetrachlorohydrate GLY Superfine Powder (REACH AZP-908) Elementis 22.00
Ingredient Supplier %w/w
Cyclomethicone (and) Dimethicone Crosspolymer 8DC 9040 Silicone Gel) Dow Corning 1.70
Ingredient Supplier %w/w
Fumed Silica (Cab-O-Sil M5) Cabot 4.30
Ingredient Supplier %w/w
Fragrance 0.50